INJECTION MOLDING ENCYCLOPEDIA
Injection Molding Encyclopedia
Find hot runner articles by industry, material, and molding defect.
Frequently Asked Questions
Find products by material
View all four productsTotal 194 articles · Current:All industries
Browse by defect, material, and industry
194 articles
When Is PEEK Required for High-Voltage Connectors on 800V Platforms?
PEEK (Victrex 650G):; melting point 343°C; long-term service temperature approximately 250°C, depending on grade; nozzle 395°C; barrel zones 375/380–385/390°C; mold temperature 170–200°C; cylinder requires 400°C. 800V primarily affects creepage distance and insulation design; long-term high-temperature performance and life margin requirements drive the switch to PEEK.
How to choose between pinpoint and side gates?
Pin-point gates are small, allow multi-point feeding, and auto-break but have high pressure loss and require three-plate molds; side gates have low pressure loss and use two-plate molds but need gate removal and leave visible marks. Compare five factors: pressure loss, gate removal, mold cost, runner waste, and appearance. Selection should prioritize appearance, then compare costs.
PPS for SMT Connectors: Warping or Brittle Fracture First?
PPS (DURAFIDE 1140A1, 40% GF): Mold temperature 150°C; melt temperature must not exceed 360°C. Pre-dry at 140°C for 3h or 120°C for 5h. Use pin-point gates φ0.8–1.2mm,. Vent groove depth: 0.005–0.008mm,. Shrinkage: 0.3%/0.8%. For small parts, the primary concern is warpage from uneven cooling and brittle fracture during assembly, not heat resistance.
How thin can LCP be for 0.35mm pitch micro connectors?
LCP (Vectra E130i, 30% GF): Melt temp 335°C, hot runner 335–345°C, mold temp 80–120°C, shrinkage 0.10%/0.40%. Achieving 0.15mm wall thickness requires injection speed filling with a fast-then-slow profile. Runner balance and vent depth are critical for yield in multi-cavity molds.
Why Choose PA9T Over LCP for Micro Connector Housings?
PA9T (Genestar G1350A, 35% GF): Melting point 300°C, Tg 125°C, water absorption 0.19%, shrinkage 0.3%/0.9%, drying 70–90°C for 4–8 hours, barrel 280–340°C, nozzle 300–350°C. PA9T is selected for housings due to its toughness, appearance, and ease of assembly, but it cannot fill walls thinner than 0.15mm..
Why Choose PPS for Micro Connectors Requiring Reflow Soldering?
PPS (DURAFIDE 1140A1, 40% GF): Mold temperature 150°C, material temperature must not exceed 360°C, nozzle 310–320°C, pin gate φ0.8–1.2mm,, vent depth 0.005–0.008mm,, shrinkage 0.3%/0.8%. After reflow soldering, re-measure dimensions, warpage, and terminal positions. PPS offers excellent thermal stability and dimensional accuracy but is brittle.
How Many Temperature Zones Are Needed for a 16-Cavity Hot Runner System?
The goal of hot runner zoning is to ensure consistent temperatures across all cavities, not necessarily one zone per cavity. Common schemes include single-zone, two-zone (inner/outer), four-zone, or one-zone-per-cavity. The number of zones depends on cavity variations and part tolerances; 16 cavities do not necessarily require 16 zones. Thermocouples must be attached to the middle section of the nozzle, not the heater.
Why Can't Naturally Balanced Runners Fill All Cavities Evenly?
Natural balance only equalizes runner lengths, not heat dissipation conditions. Artificial balance uses throttling to compensate, but throttling also causes shear heating. Judge balance by observing the melt front; three-stage short-shot testing is most efficient. Part weight variation within 2% is considered balanced.
What Is the Difference Between Series and Parallel Cooling Circuits in Multi-Cavity Molds?
In series circuits, water heats up progressively, resulting in the highest mold temperature in the last cavity; this is difficult to control for molds with more than 8 cavities. The challenge with parallel circuits is flow distribution, requiring manifolds and control valves. A common compromise is mixed series-parallel: no more than 4 cavities per string and no more than 4 strings. Cooling channels should be 15–25mm from the cavity surface.
How Do Flow and Shrinkage Change When Increasing Glass Fiber Content from 30% to 50%?
Increasing glass fiber content raises melt viscosity and reduces flow length ratio. Average shrinkage decreases, but the difference between flow-direction and transverse shrinkage increases. LCP 30% GF: 0.10%/0.40%; PPS 40%: 0.3%/0.8%; PA9T 35%: 0.3%/0.9%. Eighty percent of warpage in thin-walled long parts comes from directional differences.
Can't find the matching gate issue? Share material, part, and defect details. Our engineers will evaluate it by part.
Online selection and quote