INJECTION MOLDING ENCYCLOPEDIA
Injection Molding Encyclopedia
Find hot runner articles by industry, material, and molding defect.
Frequently Asked Questions
Find products by material
View all four productsTotal 194 articles · Current:All industries
Browse by defect, material, and industry
194 articles
Flash Causes: Parting Line, Clamping Force, and Cavity Pressure
Flash occurs when thin fins appear on edges or hard flakes form around holes and ejector pins that resist trimming. This is common in thin-wall multi-cavity parts and is directly related to gate size and holding pressure settings.
Sink Marks and Indentations: Can Holding Pressure Fill Thick Sections?
Sink marks on flat surfaces—typically at thick walls, rib roots, or bosses—cannot be concealed by polishing, as they originate from internal shrinkage.
Weld Line Formation: Confluence Point, Front Temperature, and Interface Fusion
Fine lines on part surfaces that are lighter in color and cannot be polished. These appear at hole edges, insert sides, or flow meeting points. Caused by insufficient melt temperature preventing proper fusion when two flow fronts meet.
Multi-Cavity Flow Imbalance: Simultaneous Fill
In an 8-cavity mold, outer cavities exhibit short shots while center cavities flash. Adjusting injection speed only shifts the problem location, indicating inherent flow imbalance.
Jetting Marks: Why the Initial Flow is Serpentine
Serpentine or earthworm-like patterns near the gate that fade away from the entry point, caused by jetting as the material enters the cavity.
Air Traps and Entrapped Air: Problems at the Final Fill Point
Burn marks, short shots, bubbles, or dull spots consistently occurring at part ends, weld lines, or deep cavity bottoms due to trapped air.
Insufficient Packing and Weight Instability: Once Gate Seals, Additional Pressure Is Useless
Weighing individual products from the same mold shows weight and dimension fluctuations, with occasional short shots at the end. This indicates insufficient packing and unstable weight.
Black Specks: Melt Carbonization, Residence Time, and Dead Zone Residue
Dark spots (0.x–1.x mm) on or below the surface that cannot be polished; these may appear in fixed or random locations. Often mistaken for dirt, but they persist even with new resin, indicating residue in the hot runner or screw.
Yellowing and Discoloration: Overall vs. Gate Area
Parts may exhibit overall yellowing, localized yellowing near the gate, or end-of-fill yellowing. The location indicates the root cause.
Silver Streaks and Water Marks: Gas Source and Flow Path
Silver-white streaks running along the flow direction near the gate, resembling water marks and more visible under light, caused by gas entrainment.
Can't find the matching gate issue? Share material, part, and defect details. Our engineers will evaluate it by part.